Yes, you should use ER347, please refer API 582 (Welding Guidelines for the oild and gas industries)
-- Cheers!
Raj
On Fri, Apr 15, 2011 at 1:10 PM, Bathula Raghuram (Mumbai - PIPING) <R.Bathula@ticb.com> wrote:
ER 347 is compatible fillet metal for this grade
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Zakaria ghrab
Sent: Friday, April 15, 2011 3:10 PM
To: materials-welding@googlegroups.com
Subject: [MW:10683] stainless steel Grade 321H Weldability
Hi all,
In our project we have to weld Austenetic SS grade 321H full GTAW, we used ER 308 gtaw rod filler metal, one collegue say that we must use ER 347. is it true ? use ER 308 is not compatible with these grade ?
Please help me
Regards--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments:
Post a Comment