ER 347 is compatible fillet metal for this grade
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Zakaria ghrab
Sent: Friday, April 15, 2011 3:10 PM
To: materials-welding@googlegroups.com
Subject: [MW:10683] stainless steel Grade 321H Weldability
Hi all,
In our project we have to weld Austenetic SS grade 321H full GTAW, we used ER 308 gtaw rod filler metal, one collegue say that we must use ER 347. is it true ? use ER 308 is not compatible with these grade ?
Please help me