Dear Schreedhar/ Rizal/ Shaunak Upadhyay / Prakash Hegde,
Thanks for your valuable suggestions.
-- Thanks for your valuable suggestions.
The saddle length is 200mm only, and I have suggested to use Titanium for the saddle to avoid dissimilar welding.
I think this will be the better decision to avoid carbonsteel to titanium welding problem.
Thanks and Regards,
Vijay
,
| |
,
On Tue, Apr 12, 2011 at 1:06 PM, Prakash Hegde <pb.hegde@yahoo.com> wrote:
Dear VijayTi To Cs welding is not compatableGenerally Ti lining (sheet ) is being screwed with CS, You can refer AWS welding Hand book Vol 4 for the joint configuration Which will clear your doubtsRegardsHegde P.B.
From: vijay <vijayakumarme@gmail.com>
To: weldinggang@googlegroups.com; materials-welding@googlegroups.com
Sent: Tue, 12 April, 2011 6:09:13 AM
Subject: [MW:10646] Titanium to carbon steel welding--
Dear Friends,There is a requirement mentioned in our client spec about Titanium to Carbon steel welding(Attached picture have more details).I searched for literatures on this and I found that by normal fusion welding process is not recommended.1. Is there any way,welding can be done between Titanium and carbon steel?2. If YES or NO(on both case), please send a evidence document to confirm(like ASME,ASTM).This is very urgent requirement.Thanks in advanceRegards,VijayTo post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments:
Post a Comment