I do not think so much difference in ranges of temperature hence is
U/G line .untill unless pipe will fully exposure.....
Suresh.
On 4/13/11, Nagarajan Swaminathan (Gasco - Habshan-5)
<S.Nagarajan@gascoh5.ae> wrote:
> NO MORE THAN 0.85 BAR...mathematically
>
> regards
>
> From: materials-welding@googlegroups.com
> [mailto:materials-welding@googlegroups.com] On Behalf Of SOHAIB GHNAIMAT
> Sent: Tuesday, April 12, 2011 9:13 PM
> To: materials-welding@googlegroups.com
> Subject: [MW:10655] hydro testing of Pipelines
>
>
>
>
> Team,
>
> We have just completed the hydro test for 66" underground Pipeline the
> temperature at the begining of the test / Holding time was 13 Deg C. and
> after 14 hrs of the holding period ( 24 hrs ) the temperature was 24 deg C.
>
> what will be the change in pressure ?
>
> Regards,
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>
--
Thanks & Best Regards,
Suresh
Mobile No: 91-92 92 905 905
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments: