Dear Vijay,
1. No other way for pressure vessel. you may designed short saddle made by titanium then extended by C.S support. connection by bolting.
2. -
On Tue, Apr 12, 2011 at 7:39 AM, vijay <vijayakumarme@gmail.com> wrote:
Dear Friends,--There is a requirement mentioned in our client spec about Titanium to Carbon steel welding(Attached picture have more details).I searched for literatures on this and I found that by normal fusion welding process is not recommended.1. Is there any way,welding can be done between Titanium and carbon steel?2. If YES or NO(on both case), please send a evidence document to confirm(like ASME,ASTM).This is very urgent requirement.Thanks in advanceRegards,Vijay
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
Regards,
T. Rizal Hidayat
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments:
Post a Comment