Saturday, April 9, 2011

Re: [MW:10636] ASR[AFTER STRESSRELIEVING]

Sampath Ji,
 
Did MPI carried out on weld bevel preps before welding?
Is the bevel corroded?
 
Regards,
S.SENTHILKUMAR



From: Sampath Kumar <skthatham@gmail.com>
To: materials-welding@googlegroups.com
Sent: Sat, 9 April, 2011 10:33:46 AM
Subject: [MW:10635] ASR[AFTER STRESSRELIEVING]

Dear Mr.Jaspal singh & Mr.Senthil Swaminathan,
 
The defect is in HAZ
Material:             LTCS
THICKNESS     24mm
Electroede        7018-1
Filler wire           ER70S-2
Process             GTAW/SMAW
 
Regards
sampath
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...