Tuesday, April 5, 2011

Re: [MW:10601] Weaving

The codes indirectly address weaving by making heat input an essential variable when there is a toughness requirement.

A weave 3 times electrode diameter just became a rule of thumb because it is a general rule that works well.  It is not a rule that should apply to all welding or all materials.  A welding or metallurgical engineer should be consulted to determine what limitation should be put in place.

On Apr 5, 2011 5:35 AM, "Ahmed Husain" <ahmraha@yahoo.com> wrote:

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34913] Filler wire

E71T-1C  is Charpy Impact tested at -20degC E71T-1CJ is Charpy impact tested at -40degC. AWS Classification for FCAW is only a supplementary...