Tuesday, April 5, 2011

Re: [MW:10594] UT OF PARTIAL PENETRATION JOINT OF STRUCTURAL WELD

yes ,no problem for that, what is the thickness and what is the purpose of examination to check penetration or weld quality?
regards, Bhaskar

On Tue, Apr 5, 2011 at 1:25 AM, asad azmi <azmiasadayub@gmail.com> wrote:
Dear All,
 
Greetings....
 
Is it possible to perform UT of  Partial Penetration weld joint of beam with base plate.
 
construction code is AWS D1.1.
 
Thanks and Regards 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
धन्यवाद,
भास्कर मनोहर काळे
+60149129098

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34832] Inquiry about Single Bevel with Back Grinding

Dear Uday, As per your question that one is called with backing only,Simple both side you are welding it is backing with strip or without st...