Re: [MW:10588] For 8mm/10 mm thick plate full penetration welding ,what will be the range qualified for pipe in fillet weld.

Please Refer
 
ASME Sec IX  - QW-451 Procedure Qualification Thickness Limits and Test Specimens


On 25 March 2011 11:34, Venkateswaran <k.venkateswaran@ionexchange.co.in> wrote:
 

If I conduct WPQ(SMAW or GMAW process,ASME SEC IX) for 8mm/10 mm thick plate full penetration welding ,what will be the range qualified for pipe in fillet weld.


Experts, can you Give reference clause form ASME SEC IX.


Thanks


kvr

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Thanks & Regards

Velan

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34820] RE: 34813] Clarification in Rate of heating and cooling.

Hello,   Please see the response below.   Regards.   P. Goswami, P. Eng, IWE.   From: materials-welding@googlegroups.com <materials-weld...