Hi
 
It has to specified by the contract spec.
 
Normally after root run not required incase of Structural welding by AWS D1.1, & 10% on final weld.
 
Thanks & Regards,
 
K. Babu
 

----- Original Message -----
Sent: Friday, April 01, 2011 7:35 PM
Subject: [MW:10573] DPT for Structural welding

Dear All
 
Can any body tell me if it is required to do DPT for root run & after final welding in structural steel. If yes how much percentage
 
CODE: AWS D1.1

--
Thanks & Regards
Feroz Mohammed
Deputy Manager-QA&I
LANCO Infratech Ltd.
È : +91 9650490097
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...