Re: [MW:10576] Re : Name Plate for Vessel

It should be the year when you did the final hydrotest
 


 
On Fri, Apr 1, 2011 at 4:56 AM, Vijay <k.vijayaraj@gmail.com> wrote:
Dear Mr. Mustaffi,

The name plate should have 2011 year only, we have done one vessel from sep 2010, and it completed on feb 2011, we put 2011 year only.

Regards,
Vijay


On Fri, Apr 1, 2011 at 2:05 PM, mustaffi <mustaffi@dynac.com.my> wrote:

Dear  : Experts

 

Please be confirmed , I had one vessel and HT completed on 2011 , but we make it all the progress from design till fabrication at 2010 . so the name plate need  to  register 2010 or 2011.

 

Please give me references also in ASME ..

 

TQ

 

Regards

Mustaffi Mohd

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34913] Filler wire

E71T-1C  is Charpy Impact tested at -20degC E71T-1CJ is Charpy impact tested at -40degC. AWS Classification for FCAW is only a supplementary...