Friday, April 1, 2011

Re: [MW:10571] Name Plate for ASME Vessel (year built)

Please note that the vessel is completed only all the operations including hydrostatic test is completed.
Since HT is completed in 2011, year built shall be stamped as 2011 on the name plate.
arunachalam


On Fri, Apr 1, 2011 at 2:57 PM, Bathula Raghuram (Mumbai - PIPING) <R.Bathula@ticb.com> wrote:

HT is part of fabrication, hence you should stamp it as 2011 only, code does not specify, but your AI may!

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of mustaffi
Sent: Friday, April 01, 2011 3:36 PM
To: materials-welding@googlegroups.com
Subject: [MW:10568] Re : Name Plate for Vessel

 

Dear  : Experts

 

Please be confirmed , I had one vessel and HT completed on 2011 , but we make it all the progress from design till fabrication at 2010 . so the name plate need  to  register 2010 or 2011.

 

Please give me references also in ASME ..

 

TQ

 

Regards

Mustaffi Mohd

 


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Arunachalam.A, ME
Abu Dhabi Gas Industries Ltd,
P.O.Box # 50124
Abu Dhabi, UAE
Mobile : +971-50-5257122

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3