Re: [MW:10567] saw wire & flux

Dear Pawan,


You can use AWS SFA 5.23 (3NiCrMo2.5) Filler Wire and Flux Both. 


On 1 April 2011 14:22, pawan <pawan.tiwari@dwekam.org> wrote:

Dear Experts,

Kindly suggest suitable saw wire & flux combination for SAILMA 550HI GR steel (for PAN STOCK FABRICATION). The plate thickness is around 20-70mm.

 

Thanks & Rgd

Pawan Tiwari

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



Regards

K U Masood Ahmad

Industrial Services
SGS India Private Limited
Himachal Sorang H.E.P.
GSM +91 - 9805997411

ku.masoodahmad@sgs.com

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...