Friday, April 1, 2011

Re: [MW:10565] Re : SA 240 316L for AWS D1.1

Hi,
Pls.refer AWS D1.6 for Structural Welding-Stainless steel. as specified in AWS D1.1 - 1.2 (4).
Pls.find below the extraction.

(4) Base metals other than carbon or low-alloy steels.
AWS D1.6, Structural Welding Code—Stainless Steel,
should be used for welding stainless steel structures. Whenever
contract documents specify AWS D1.1 for welding
stainless steel, the requirements of AWS D1.6 should apply.

Thanks & Regards,

(Karthik)

Karthikeyan.S
QA/QC Manager
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282


--- On Fri, 4/1/11, mustaffi <mustaffi@dynac.com.my> wrote:

From: mustaffi <mustaffi@dynac.com.my>
Subject: [MW:10563] Re : SA 240 316L for AWS D1.1
To: materials-welding@googlegroups.com
Date: Friday, April 1, 2011, 3:49 PM

Dear All

 

Please help me for this question, SA 240 316L for AWS D1.1  which references group of materials

 

Regards

Mus

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34820] RE: 34813] Clarification in Rate of heating and cooling.

Hello,   Please see the response below.   Regards.   P. Goswami, P. Eng, IWE.   From: materials-welding@googlegroups.com <materials-weld...