Hi,

Method is not a matter,
The values are important,
 if ur old values satisfy with new requirement then no need go for A new PQR.

Tnks



On Thu, Mar 31, 2011 at 3:47 PM, vijay kumar <vijaykumaar80@gmail.com> wrote:
Dear all
 
We have a previous project qualified welding procedure, but hardness test carried out in old method in that pqr, present project spec is saying that requirement of test as per NACE MR0715 ISO 15156. i have some doubts about it
 
we can weld a coupon as per wps and do the hardness test as per nace requirment or need to qualify newly with all tests
pls send the reply with code reference
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...