[MW:10848] Multi and Single Pass fillets-ASME Sec IX

Dear All

According to ASME sec IX, for GTAW, FCAW and GMAW in supplementary essential variables (QW 410.9) , a multi pass per side fillet/butt weld procedure cannot be used to weld single pass per side. (say single pass per side fillet weld.)
I am curious to know the technical reason behind the same. In my opinion, fill pass parameters of a butt weld procedure can be used for welding single pass fillet welds. Please advice if this is incorrect and kindly provide technical/ metallurgical reasoning for the same.

Thanks & best regards

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34874] ASME IX, groove weld during WQT limits for Fillet Weld production

Hi David,  There are two points in WQT. 1. Thickness of Base Metal -T 2. Thickness of Weld Metal -t When you use a combination of two proces...