Hi all,

  We have a PQR, 15 mm Thickness, welded 6mm GTAW, 9mm SMAW.
According ASME sect IX, table QW-451.1, the Qualified Thickness "T" of base metal qualified will be 1.5 mm to 30 mm and the deposit weld thikness GTAW will be 12 mm max "2xt".
 Means if i have to weld pipe thick 3 mm i can't use this PQR, i'm right ?

--
زكرياء غراب


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...