Hi,

For E7018, the typical storage and drying conditions is mentioned in
Table 'A3" of Section II Part'C'. For SS it is not mentioned
specifically in Sec II part'C', but in BS EN 1011-3 it was mentioned
as "covered electrodes should be re-backed before welding, if
necessary, in accordance with the manufacturer's/supplier's
recommendations."

Cheers!

Raj


On Apr 21, 4:16 pm, Rodrigo <rpcu...@firjan.org.br> wrote:
> I would like to help one of their colleagues in relation to compulsory
> treatment for drying of coated stainless steel electrodes (E316L) as
> well as the electrodes type E7018. There is a bibliography of ESAB
> determines that such treatment at 225 ° C for 1.5 hours. Someone could
> tell me if it proceeds? Or just be a good practice of drying the
> welding consumables?
>
> Thanks
>
> Rodrigo Fernandes Rodrigues Pimenta da Cunha Eyer
> Centro de Tecnologia SENAI-RJ Welding
> tel. 55 (21) 3978-8703 / 9407-9355
> FIRJAN -www.firjan.org.br

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...