[MW:10796] Izod test temp for EN19 steel

Dear Friends

I wanted to use EN 19 plate in one of my present project, wherein the application demands severe impact loads at room temperature.

I had browsed through the properties of EN 19 plate in various literatures wherein the Izod test values are mentioned @ 55J.

However the Izod testing temperature is not mentioned.

Can anyone help me out or guide me where to refer, so that i can know the Izod testing temperature of this EN 19 steel.

Secondly i would also like to know which of the two will have more toughness and why - EN 19 casting OR EN19 plate ?
The reason being the final component will have to be casted due geometrical complications.


Regards

Prem Nautiyal



PREM S NAUTIYAL
CELL : 9769316004

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34913] Filler wire

E71T-1C  is Charpy Impact tested at -20degC E71T-1CJ is Charpy impact tested at -40degC. AWS Classification for FCAW is only a supplementary...