Thursday, April 21, 2011

[MW:10777] Reg:filler wire for dissimilar material

dear experts,
good day all of you.
i need your valuable help: 
which filler wire we can use for dissimilar metals in heater piping
1. ASTM A335 Gr. P9 (9 Cr,1 Mo ) half coupling to ASTM A 240 Gr 310 plate fillet weld.
2. ASTM A335 Gr. P9 (9Cr, 1 Mo ) coil  to ASTM A 351 Gr.HK 40 plate

PL suggest me

thanks & regards


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34832] Inquiry about Single Bevel with Back Grinding

Dear Uday, As per your question that one is called with backing only,Simple both side you are welding it is backing with strip or without st...