[MW:10764] RE: 10752] SIngle procedure

Hello Fredric,

This is not a problem when you perform all required tests for both
specifications on the test piece.
This means NDT has to be performed according to both ASME and EN codes and
you need separate NDT reports for each specification. But also different
tensile specimens need to be taken from the test weld because of different
size of these specimens according to the specifications.
In the past we performed procedure testing with only one set (2 pieces) of
Cross Weld tensile specimens according to EN specification because these are
wider than the ASME specimens. Because of an unknown reason today this is
not longer accepted by notified bodies which in my opinion is completely
stupid. Specimen wide for EN is 25 mm and for ASME 19 mm for Cross Weld
tensile specimens. Looking to the results there is no big difference between
both. Hopefully this problem will be solved by the next generation of the
EN-ISO 15614-1 which will become available soon.
You need to prepare you pWPS also in such way that all essential parameters
for both specification are mentioned on this document.

Met vriendelijke groeten / Best Regards

Herman Pieper

Pieper Quality Support & Inspection
Phone: +31 (0)521 380083
Fax: +31 (0)84 7539225
Cell: +31 (0)6 51691215
www.pieper-qsi.nl

-----Oorspronkelijk bericht-----
Van: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] Namens fredric prabu
Verzonden: woensdag 20 april 2011 6:56
Aan: materials-welding@googlegroups.com
Onderwerp: [MW:10752] SIngle procedure


Hello

Can somebody advice if we can make a single procedure covering both ASME and
EN Specs in SMAW process

Thanks

Regards
Fredric

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and
meant for educational purposes only, Users must take their own decisions
w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...