[MW:10746] Re: WQT

Hi,

You question is not clear?

6GR shall be qualified as per Figure 4.27 of AWS D1.1 with a minimum
thk of 12mm for dia 6" and above.

Let me answer in a generic way!

A) If a WQT is conducted on a 6" Dia x 12mm thk pipe in 6GR position
(as per Figure 4.27 of AWS D1.1) - The qualification range for the
welder will be

1) Can weld (Butt Groove) All CJP, PJP except mentioned in the
brackets (Not qualified for joints welded from one side without
backing, or welded from two sides without back gouging) - Refer Table
4.10 for more details.
2) Can weld (T, Y, K Groove) All CJP, PJP except mentioned in the
brackets (Not qualified for welds having groove angles less than
30deg) - Refer Table 4.10 for more details.
3) Nominal Pipe Size Qualified - 4" and above
4) Nominal Pipe Thickness Qualified - 5mm and above
5) Dihedral Angles Qualified - 30deg and above.


B) If a WQT is conducted on a 6" Dia x 11mm thk pipe in 6G position -
The qualification range for the welder will be

1) Can weld (Butt Groove) All CJP, PJP
2) Can weld (T, Y, K Groove) All PJP
3) Nominal Pipe Size Qualified - 4" and above
4) Nominal Pipe Thickness Qualified - 5mm and above

Hope the above will guide you something!

Cheers!

Raj

On Apr 19, 6:30 am, kalimuthu ponniah <kalimuthu.ponn...@gmail.com>
wrote:
> Dear Friends,
> WQT was conducted on pipes 6GR position with 6" wall thickness 11mm.
> As per AWS D1.1 table 4.11, does the welders qualify? Please advice me which
> one to follow(Production CJP Groove Butt Joints or Production T-Y-K
> Connections CJP Groove Welds)
> Do I have to re qualify the welders? Our production pipe is 12"OD X 25.4mmWT
> and 8"OD X 20.6mmWT. Your kind cooperation on the above is highly
> appreciated.
>
> Regards,
> KalimuthuPonniah.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...