[MW:10740] Re: Welding of two different Group metal (Gr II with Gr III)

dear all,

AS per AWS, WPS is not possible..
in aws d1.1, table 4.12, group number & p number is not an essential
variable for welder qualification.
by this table its possible..
am i right..
if wrong correct me.