Hi,

AWS D1.1 is not specifically mentioning about combining of two or more
PQRS.

If you refer table 4.8 of AWS D1.1, It specifies as If PQR base
material used is "Any Unlisted steel to Any Unlisted steel or Any
steel listed in table 3.1 or Table 4.9" - WPS base metal group
combinations allowed by PQR will be "Only the specific combination of
steel listed in PQR".

Since grade S355JR is belongs to BS standard and according AWS D1.1
table 3.1/4.9, this material shall be considered as "Un Listed".

You cannot club these two PQRs for welding each other. You have to
qualify a PQR with a combination of "S355 JR to Group III" material.

Hope this will clarify.

Cheers!

Raj

On Apr 18, 5:54 pm, Brl Pp <refazosa...@gmail.com> wrote:
> Good morning,
>
> Please advise us if the welding of two different Group metal (Gr II
> with Gr III) is covered by the PQRs of both groups, according to AWS
> D1.1 code.
>
> Example:
>
> PQR1: concern the welding of S355 JR - S355 JR (Gr II)
>
> PQR2: concern the welding of API 5L X60 - API 5L X60 (Gr III)
>
> Question: The welding of S355 JR - API 5L X60 is covered by the above
> PQR (PQR1 & PQR2) according to AWS D1.1 code?
>
> Thank's and regards
> REDOUANE

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...