Hi,

No, there is no mandatory requirements regarding 'calibration
certificates', 'prescribed height for fixing test coupon' for welder
qualification as per AWS D1.1 or ASME Sec-IX.

Cheers!

Raj

On Apr 18, 7:07 am, SENTHIL P <senbe...@gmail.com> wrote:
> Dear sir,
>     i wish to know the general procedure for welder
> qualification.e.g calibration certificate .is any precribed height for
> fixing test piece for qualification. please clarify.
>
>  thank u,
>  sen

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...