The PQP describes all general items related to the project in detail such as
applicable codes, requirements for the execution of welding, materials and
material certificated and requirements for fabrication such as Non
Destructive Testing (NDT).
The QIP also called ITP (Inspection % Test Plan) is more a check list which
describes all the moments in the production process where quality actions
need to be executed in front of or during production, such as review of
material certificates, review of PQR / WPQ and WPS documentation and
describes also who is responsible for it and if it is a hold point,
witnesses point or monitoring point for companies own QA/QC department,
Clients representative and/or Certifying Authority / Notified body.
Met vriendelijke groeten / Best Regards
Herman Pieper
Pieper Quality Support & Inspection
Phone: +31 (0)521 380083
Fax: +31 (0)84 7539225
Cell: +31 (0)6 51691215
www.pieper-qsi.nl
-----Oorspronkelijk bericht-----
Van: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] Namens aslam khan
Verzonden: zondag 17 april 2011 7:59
Aan: materials-welding@googlegroups.com
Onderwerp: [MW:10695] what6 is difference between QIP AND PQP
hi friends,
dear friends ,what is difference between QIP(quality inspection plan)
and PQP(project quality plan )? thanks in advance .
best regards
ASLAM
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and
meant for educational purposes only, Users must take their own decisions
w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments:
Post a Comment