Sunday, April 17, 2011

[MW:10690] RE: 10688] ABS GR, AH-36 MATERIAL

Hello Bhaskar,
 
You may please refer ASTM-A-131-Standard Specification for Structural Steel for Ships. This steel is classified as:-
  • Higher Strength—Grades AH, DH, EH, and FH with a specified minimum yield point of 46 ksi [315 MPa], 51 ksi [350 MPa], or 57 ksi [390 MPa].
Thanks.
 
Pradip Goswami,P.Eng.IWE
Welding & Metallurgical Specialist & Consultant
Ontario,Canada.
Email-pgoswami@sympatico.ca,
 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of bhaskar rao
Sent: Saturday, April 16, 2011 2:54 AM
To: materials-welding@googlegroups.com
Subject: [MW:10688] ABS GR, AH-36 MATERIAL

Dear friends,
 
Please give me the reply for ABS GR,AH-36 Equalent material in
 ASME or ASTM.
 
Regards,
 
PBRAO,

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...