[MW:10655] hydro testing of Pipelines




Team,
 
We have just completed the hydro test for 66" underground Pipeline the temperature at the begining of the test / Holding time was 13 Deg C. and after 14 hrs of the holding period ( 24 hrs ) the temperature was 24 deg C.
 
what will be the change in pressure ?
 