Dear All,
We have 32 frame (Square Flanges) with following dimension 75*2500*3400 mm and the material is SA516 Gr 70 ( PNo.1) each one have 4 welding line at the corner with length 110 mm , PWHT for this item is suggested to be local the question is
If we make PWHT by furnace is there any problems related to this? and what are this problems?
--
Best Regardes,
Eng:- Elsayed Elghareeb.
Dipl. Welding Engineer.
+2 010 82 61 645.