Dear Friend,
Can you tell me the equivalent material of construction for the following Chinese Pipe & tube.
- 20G
- 20G+15NiCuMoNb564
- 15CrMoG+20G
- 15CrMoG+12Cr1MoVG
- 12Cr1MoVG
- 20G+12CrMoVG
- 12Cr1MoVg+SA182-F22
- 12Cr1MoVG+SA217WC6
- 20/WCB
- 1Cr18Ni9Ti
- 20G+SA106B.
Thanking You.
Regards
Sachin Shelar
Sr. Engineer - Process Engg
Thermax Ltd.
Ph +91 20 66126775
E Mail: sachin.shelar1@thermaxindia.com
================================================================================================================
DISCLAIMER by THERMAX LIMITED
The information in this email is confidential and may be legally
privileged.It is intended solely for the addressee. Access to this email by anyone else is unauthorized.If you are not the intended recipient, any disclosure, copying, distribution or any action taken or omitted to be taken in reliance on it, is prohibited and may be unlawful. When addressed to our clients any opinions or advice contained in this email are subject to the terms and conditions.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments:
Post a Comment