Tuesday, April 12, 2011

[MW:10651] RE: 10646] Titanium to carbon steel welding

Dear Vijay,

 

Why full titanium plate is used for shell. Often explosive cladded carbon steel is used. In such case you will have an Titanium liner inside and the outside is Carbon Steel so will not have any problems to connect any saddles and or other attachements.

 

Met vriendelijke groeten / Best Regards

 

Herman Pieper

 

Pieper Quality Support & Inspection

Phone: +31 (0)521 380083

Fax:     +31 (0)84 7539225

Cell:     +31 (0)6 51691215

www.pieper-qsi.nl

 

Van: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] Namens vijay
Verzonden: dinsdag 12 april 2011 2:39
Aan: weldinggang@googlegroups.com; materials-welding@googlegroups.com
Onderwerp: [MW:10646] Titanium to carbon steel welding

 

Dear Friends,

 

There is a requirement mentioned in our client spec about Titanium to Carbon steel welding(Attached picture have more details).

I searched for literatures on this and I found that by normal fusion welding process is not recommended.

1. Is there any way,welding can be done between Titanium and carbon steel?

2. If YES or NO(on both case), please send a evidence document to confirm(like ASME,ASTM).

This is very urgent requirement.

 

Thanks in advance

 

Regards,

Vijay

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34913] Filler wire

E71T-1C  is Charpy Impact tested at -20degC E71T-1CJ is Charpy impact tested at -40degC. AWS Classification for FCAW is only a supplementary...