procedure Qualification as per API 1104 Dia Range Is essential Variable or non?
 
api 1104 5.3.2.3 is showing that need to specify diameters and wall thickness in wps but Essential Variables (5.4) doesn't Say's that dia range
 
waiting for valuable replays
 
thnks

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.