Can you give some more information
What is the material ?
What is base metal Thickness?
Consumable Used?
Welding Process?
Regards
Jaspal Singh
Quality Assurance
ISGEC-YNR
9996624244
On Mar 26, 10:18 am, Sampath Kumar <skthat...@gmail.com> wrote:
> Dear Experts,
>
> One joint we found some base metal defects[A sort cluster pore]which is
> slightly away from the weld metal.can we grind and check.please suggest what
> kind of corrective action to be taken with valid reasons.Also please let me
> know "DOS & DONT'S AFTER PWHT".
> With Best Regards
> Sampath
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments:
Post a Comment