[MW:10592] UT OF PARTIAL PENETRATION JOINT OF STRUCTURAL WELD

Dear All,
 
Greetings....
 
Is it possible to perform UT of  Partial Penetration weld joint of beam with base plate.
 
construction code is AWS D1.1.
 
Thanks and Regards 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3