Dear all,

We have 2 API storage tanks,with dimensions & drain nozzle sizes as
follows,

Tank 1 - ID 6000 x Ht 9500 , Drain Nozzle NPS 4

Tank 2 - ID 3000 x Ht 3000 , Drain Nozzle NPS 2

Licensor Datasheet has asked to, "PROVIDE FLUSH DRAIN WITH BOTTOM OF
TANK AS PER API650".

However, API 650 gives details for nozzles NPS 8 & above.

Please guide me for above cases.

regards,
Mandar Kardekar
Mechanical-Stationary Engineer


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34874] ASME IX, groove weld during WQT limits for Fillet Weld production

Hi David,  There are two points in WQT. 1. Thickness of Base Metal -T 2. Thickness of Weld Metal -t When you use a combination of two proces...