Friday, April 1, 2011

[MW:10573] DPT for Structural welding

Dear All
 
Can any body tell me if it is required to do DPT for root run & after final welding in structural steel. If yes how much percentage
 
CODE: AWS D1.1

--
Thanks & Regards
Feroz Mohammed
Deputy Manager-QA&I
LANCO Infratech Ltd.
È : +91 9650490097
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...